Product specifications:
Size DN/ID | Pipe Inner Diameter d≥ | Pipe OD de≥ | Depth of the socket Ls≥ | Socket diameter D≥ |
200 | 195 | 226 | 150 | 242 |
225 | 221 | 260 | 150 | 260 |
300 | 296 | 338 | 153 | 342 |
400 | 392 | 458 | 230 | 463 |
500 | 491 | 578 | 260 | 563 |
600 | 595 | 695 | 220 | 665 |
800 | 785 | 910 | 220 | 890 |
Comprehensive comparison between PE double - walled tube and other tubes | |||
Items | PE double wall bellows | PVC-U | Coagulation and tube |
corrosion resistance | 在海水及酸、堿士壤中不會(huì)被腐蝕,抗酸堿腐蝕能力強(qiáng) | 較好 | 不耐酸喊腐蝕,嚴(yán)重者將產(chǎn)生泄露告成地下水污染 |
impact resistance | 耐中擊性好 | 在硬物沖擊下有破裂、短裂危險(xiǎn),耐中擊性差 | 較好 |
Flexibility | Good flexibility, seismic section uneven settlement when not broken, suitable for any soil | Better | not good |
application property | Saving mechanical cost, convenient connection, guaranteed construction quality in winter (minimum construction temperature up to minus 30°C), good construction, especially suitable for northern China | Rubber sealing ring or adhesive connection is adopted, which is convenient for construction but difficult to ensure the construction quality in winter (minimum construction temperature 5°C) | Heavy material, inconvenient transportation construction, poor manual connection |
Economy | The comprehensive cost is low | The comprehensive cost is low | Low cost of materials but high cost of operation and maintenance |
sanitary property | Non-toxic and pollution-free, sanitary property as the best | When the waste pipe is burned, it will release heavy metal smoke and pollute the environment | There will be leakage phenomenon, pollution of the environment |
Service life | More than 50 years | 50 years | 10-20 years |
Performance index of polyethylene (PE) double wall bellows | ||
Items | performance evaluation | |
Appearance | Obvious impurities and irregular ripples in the inner and outer walls of the pipe are not allowed. Both ends of the pipe should be flat and perpendicular to the axis and located in the trough area of the pipe. The inner and outer walls of the trough area of the pipe should be fused tightly, and it is not easy to break away | |
ring-stiffness,KN/m | SN4 | ≥4 |
SN8 | ≥8 | |
Flexible ring | The specimen is smooth, no reverse bending, no rupture, no separation of the two walls | |
Oven test | No bubbles, no delamination, no cracking | |
Impact Testing,(TIR )/% | ≤10 | |
Creep Rate | <4 |